ASTM B443 Alloy 625 / UNS N06625 Nickel Alloy Steel Sheet / Plate
1. Grade: Alloy 625, Alloy C276/N10276, Alloy C-4/ UNS N06455, Alloy B/UNS N10001, Alloy B-2/UNS N10665, Alloy B-3/UNS N10675, Alloy C22/UNS N06022, Alloy 800/N08800, Alloy 825/N08825, Alloy 400/N04400; etc
2 . Length : As customer's requirement
3 . Standard : ASTM B333; ASTM B575; ASTM B168; ASTM B443; ASTM B670 etc.
4. Technology : Cold Drawn / Cold Rolled
Chemical composition
% | Ni | Cr | Mo | Fe | C | Mn | Si | P | S | Co | Nb+Ta | Al | Ti |
min | 58.0 | 20.0 | 8.0 | 3.15 | |||||||||
max | 23.0 | 10.0 | 5.0 | 0.10 | 0.50 | 0.50 | 0.015 | 0.015 | 1.00 | 4.15 | 0.40 | 0.40 |
Physical properties
Density | 8.44 g/cm3 |
Melting range | 1290-1350℃ |
Features: Alloy 625 has excellent strength at temperatures up to 816℃. At higher temperatures, its strength is generally lower than that of other solid solution strengthened alloys. Alloy 625 has good oxidation resistance at temperatures up to 980℃ and shows good resistance to aqueous corrosion, but is relatively moderate compared to other more capable corrosion resistant alloys.
Applications: Chemical process industry and sea water application. Alloy 625 is used in short term applications at temperatures up to 816℃. For long term service, it is best restricted to a maximum of 593℃, because long term exposure above 593℃ will result in significant embrittlement.