TP309s / 310s Stainless Steel U Bend Heat Exchanger Tube, ASTM A269 Welded Tube For Boiler
SSHEWT12
Material: 309/309S/309H, 1.4833; 310/310S/310H,1.4845;
Get QuoteTP309s / 310s Stainless Steel U Bend Heat Exchanger Tube, ASTM A269 Welded Tube For Boiler
Our heat exchanger tube with pickling and annealing surface is very popular in boilers and heat exchangers industry , water heater industry , air-conditioning industry etc . This kind of seamless tubes are have a very important position in our all products .
Chemical Composition :
Material | ASTM A269 Chemical Composition % Max | ||||||||||
C | Mn | P | S | Si | Cr | Ni | Mo | N B | Nb | Ti | |
TP304 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-11.0 | ^ | ^ | ^. | ^ |
TP304L | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-12.0 | ^ | ^ | ^ | ^ |
TP316 | 0.08 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 10.0-14.0 | 2.00-3.00 | ^ | ^ | ^ |
TP316L | 0.035 D | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 10.0-15.0 | 2.00-3.00 | ^ | ^ | ^ |
TP321 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | 9.0-12.0 | ^ | ^ | ^ | 5C -0.70 |
TP347 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | 9.0-12.0 | 10C -1.10 | ^ |
Grade:TP 304; TP304H; TP304L; TP316; TP316L; TP 321;TP321H; TP317L; TP310S; TP347H
Standard:ASTM A213, ASTM A 269, ASTM A 270,EN10216-5; ASTM B 622;ASTM B516;ASTM A789, etc
Size: OD:3.18-101.6mm
WT:0.5-20mm
Length: Max.12M
Application
a) For fluid & gas transport
b) Structure & machining etc
Advantages
a) Advanced technology of cold draw machine
b) Advanced annealing machine
c) Better mechanical property
d) More precise dimension
e) Perfect inspection method and inspection equipment etc
Process :
1 . We use Cold Drawn techonology to produce U bend tube
2 . U bend tubes produce will accordance to customer's drawings
3 . To avoid oxidation , inert gas (Argon) is passed through tubes ID at the required flow rate
4 . The radius is checked for its OD and wall thinning with the recommended specification
5 . We'll choose three different position or as customer's require to make sure tubes quality . We'll do physical properties and micro-structure test
6 . Visual inspection for waviness and cracks is done with Dye Penetrant Test
7 . Each tube is then hydro tested at the recommended pressure to check for leakage