TP316L U Bend Tube With Low Price, Heat Exchanger Tube
SSHE01
Price: From $4500-9000USD/TON
Material: 316L, 1.4401, 1.4404, 1.4435;
Get QuoteTP316L U Bend Tube With Low Price, Heat Exchanger Tube
Our heat exchanger tube with pickling and annealing surface is very popular in boilers and heat exchangers industry , water heater industry , air-conditioning industry etc . This kind of seamless tubes are have a very important position in our all products .
Chemical Composition :
Material | ASTM A269 Chemical Composition % Max | ||||||||||
C | Mn | P | S | Si | Cr | Ni | Mo | N B | Nb | Ti | |
TP304 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-11.0 | ^ | ^ | ^. | ^ |
TP304L | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 8.0-12.0 | ^ | ^ | ^ | ^ |
TP316 | 0.08 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 10.0-14.0 | 2.00-3.00 | ^ | ^ | ^ |
TP316L | 0.035 D | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 10.0-15.0 | 2.00-3.00 | ^ | ^ | ^ |
TP321 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | 9.0-12.0 | ^ | ^ | ^ | 5C -0.70 |
TP347 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | 9.0-12.0 | 10C -1.10 | ^ |
ASTM A213 / A213 M | ||
Elements | 304L(wt%) | 316L (wt%) |
(C) Carbon, max | 0.035 | 0.035 |
(Mn) Manganese, max | 2 | 2 |
(P) Phosphorus, max | 0.045 | 0.045 |
(S) Sulfur, max | 0.03 | 0.03 |
(Si) Silicon, max | 1 | 1 |
(Ni) Nickel | 8.0 - 12.0 | 10.0 - 14.0 |
(Cr) Chromium | 18.0 - 20.0 | 16.0 - 18.0 |
(Mo) Molybdenum | N/A | 2.0 - 3.0 |
(Fe) Iron | Bal. | Bal. |
(Cu) Copper | N/A | N/A |
(N) Nitrogen | N/A | N/A |
Process :
1 . We use Cold Drawn techonology to produce U bend tube
2 . U bend tubes produce will accordance to customer's drawings
3 . To avoid oxidation , inert gas (Argon) is passed through tubes ID at the required flow rate
4 . The radius is checked for its OD and wall thinning with the recommended specification
5 . We'll choose three different position or as customer's require to make sure tubes quality . We'll do physical properties and micro-structure test
6 . Visual inspection for waviness and cracks is done with Dye Penetrant Test
7 . Each tube is then hydro tested at the recommended pressure to check for leakage